Inquiry (采购产品): Quote Request We have 4” x 4” molybdenum plates for grinding top and bottom. These plates are used in a high temperature kiln operation and become warped and out of flat with use. We need a minimum of 3.25 sq inches of surface ground flat on both sides. The thickness of the plates currently runs between .080 and .120. In our experience about .005 of material will have to be removed from both sides. However the overall thickness of the plates cannot drop below .070. The plates are in lots of approximately 100 pieces and several lots are ready for grinding. This will be a continuing periodic requirement. **** Hidden Message ***** Robert Caesar 61 Union St Attleboro, MA 02703 USA Company: Composite Modules, Inc Phone: 508-226-0420 Fax: 508-226-0938 E-mail: bc@cmodules.com **** Hidden Message ***** bc@cmodules.com