Hi! Material of the screw is steel 35 (i.e. 0.35% of carbon) Tolerance: for a billet +/- 0.15 mm; precision with which a billet should be put into the stamp: 0.1 mm A billet must be heated to the temperature of 1200 degrees Celsius, no heat treatment is expected. No requirements for the hardness. UT test is not needed. The cycle of stamping is 5 seconds, of which 2 s for the press work, 3 s for the robot-manipulator work. Price limits: USD 40 000 for robot-manipulator, USD 50 000 for press. The screw is absolutely ready after stamping and thread rolling, no additional operations are expected. Yours very truly, Sieva fti@tut.by 这个人是白俄罗斯的,不过她的英语还是可以的 附件过大,有要的可以联系我 1464272440