Inquiry (采购产品): Solvent based HAA What are the requirements for the temperature of the product for application on a grauvre printer. I have had the experience that occasionally a fininshed product left unconverted for a few days will start sticking together. I am unsure if this is a drying issue or a blocking issue. Is a cooling of the substrate nessasary after application? This is in reference to PVC film that has had an application of an HAA product and not been converted into a sleeve. I have been told by a few Grauve press operators that the COF of the finished product also seems to change from roll to roll. What would cause such a fluctuation? This is a product line we would like to explore. It seems like the unknown and other variables are dishearting. What would you recommend as far as where to obtain additional information on sustianed temperature requirements, equipment for regulating consistant ink pot temperature, drying settings, high COF problems ect.? **** Hidden Message ***** Lilian Logan PO Box 130 Dunkirk, NY 14048-0130 USA Company: Ultrapak Title: Production/QC Manager Phone: 1-800-228-6030 Fax: 1-716-366-0041 E-mail: lilian@ultrapak.us **** Hidden Message ***** lilian@ultrapak.us