Inquiry (采购产品): Krylon Indoor/Outdoor spray enamel I have had a problem twice now with your indoor/outdoor gloss aerosol enamel. When applied wet the surface looks even, free of overruns, etc.. But, as it dries the surface either wrinkles into a rough scaly-like surface or into huge wrinkles an eigth inch high. What is my problem and how do I solve it? How big a factor is it with temperatures in the 60 degree range? Thank you. **** Hidden Message ***** Jack Greenfield 1968 Dunloe Circle Dunedin, FL 334698 USA Company: None Title: Dr. Phone: (727) 734-4141 Fax: None E-mail: jegreenfield@verizon.net **** Hidden Message ***** jegreenfield@verizon.net